Job Recruitment Website - Zhaopincom - Rongjue Beauty Cream comes out very slowly.

Rongjue Beauty Cream comes out very slowly.

1, the construction interval is too long: if the time interval between the first sealant and the second sealant is too long (for example, more than 30 minutes), it may be semi-cured or solidified, and then the glue nozzle will be blocked, making it difficult to discharge the glue. In this case, a new mixing nozzle can be replaced.

2. Viscosity increases at low temperature: As the caulking agent is a polymer material, it is usually constructed in cold winter, and the external environment temperature is low, so the viscosity will increase and it is not easy to bond. At this time, we can put the caulking agent in hot water for preheating to reduce the bonding resistance.

3. The rubber nozzle cut is too small: if the opening at the front end of the mixing tube is relatively small, the discharging will be slow and laborious.

4. Wrong choice of glue gun: Generally, the glue gun of glass glue is weak, which will also cause construction difficulties, so choose the correct glue gun.

5. Incorrect installation of the glue gun: the hose is not aligned with the glue gun, and the stress on the hose is uneven, so it is also important to install the glue gun correctly.

6. The quality of the glue gun is not enough: if the quality of the glue gun is poor, the pressure it can bear is limited. When the pressure of the glue gun is too low, the feel of the glue gun will be very soft, and sizing will certainly be more difficult.