Why is the aluminium scrap granular when turning the end face? Would you please ask the lathe master to help you solve it?
The aluminum material is soft, if the cutter is not sharp enough, the rake angle is too small or the cutting speed is too low, and the amount of feed-back cutter is too small, the chips may be unsmooth and granular. In this case, a sharper knife, deeper cutting depth or higher cutting speed can all be improved. There is also a small feed.
- Related articles
- Brief introduction of Jiangmen Yidu Semiconductor Co., Ltd.
- 20 19 comprehensive knowledge questions of teacher recruitment examination (multiple choice questions)
- What are the large recruitment websites in China?
- What is the telephone number of Chongqing Kaide Jiuzhang Marketing Center?
- Which technical school in Changchun learns CNC milling machine?
- What is the relationship between Henan Mobile and Henan Sinoe?
- Where is the interior design training in Nanning?
- What is the treatment of Saint Seth-Rong Tai (Yangzhou) Precision Die Casting Co., Ltd.?
- All information about Lingxi Town, Cangnan, Wenzhou
- Announcement of 20 12 open recruitment of primary school teachers in Baohe District, Hefei City, Anhui Province