How to dry printed thick plate net? Under the guidance of a master!

Are you using water-based thick glue? The red one takes longer to expose. If the flowers wash away, it means you don’t have enough exposure time. The thick red adhesive glue is very dry, so you need to soak it in water for about half an hour after exposure. The maximum thickness cannot exceed 0.5MM. You can try the one from our factory, which is blue and water-based thick version. Don’t make the printing surface too thick. Make the thickness on the exposed surface. Generally, it will be very thick after about eight strokes (about four or five strokes at a time)