The bending angle of the electroslag pressure welding joint shall not be greater than 3, and the axis deviation shall not be greater than 0. 1 times the diameter of the steel bar, and shall not be greater than 2mm.

The visual inspection of electroslag pressure welding head shall meet the following requirements:

1, the height of the peripheral welding package protruding from the steel surface shall not be less than 4 mm.

2, steel contact with the electrode, there should be no burn defects;

3. The bending angle of the joint shall not be greater than 3;

4, the axis of the joint offset shall not be greater than 0. 1 times the diameter of the steel bar, and shall not be greater than 2 mm ..

(1) Arc welding head:

The weld surface of 1 shall be smooth, concave or shiny.

2 There shall be no cracks in the joint area.

3. The depth of lateral undercut is not more than 0.5 mm, the number of air holes with a weld surface length of 2d is not more than 2, and the slag inclusion area is less than 6 mm2.

4. The joint axis deviation is not more than 0. 1d or 3mm, and the bending angle is not more than 7/ 100 (4).

(2) Electroslag pressure welding head:

The axis deviation of 1 is not more than 0. 1d or 2mm, and the bending angle is not more than 7/ 100 (4).

2 The welding package around the joint should be uniform without cracks, and the height of the steel bar surface should be greater than 4 mm ..

3 steel surface should have no obvious burn defects.